LOWER GLOSS DARK CHARCOAL FINISH, WILL HAVE A METALLIC LOOK IN SUNLIGHT AS PICTURED BELOW. -
GOOD THERMAL/CORROSION RESISTANCE. -
CERAMIC PRIMER CAN BE USED IN COMBINATION WITH GRAY ICE FOR ADDITIONAL HEAT RESISTANCE. -
INSTRUCTIONS ON USE:
-
Follow normal ceramic prep procedures. -
Prior to spraying blast with Black Beauty, Aluminum Oxide, or sand for prep (DO NOT USE GLASS BEAD). -
Wipe down thoroughly with acetone or MEK only and let evaporate completely. Do not use chemical degreasers/phosphatizers. -
Place in oven at 450F for 1 hr, remove and let cool. -
Apply coating with airbrush or .6-.8mm tip touch up gun. This should be done at 35-40 lbs of air pressure. -
Let parts air dry 30-60 minutes. -
Recommended cure in oven at 750F for 1 hr OR follow steps 8 & 9. -
Cure in oven at 450F - 500F for 1 hr. This is a partial cure at 450-500F that will allow the part to be handled for installation. -
Once parts are installed, take vehicle for a light drive allowing the engine to get up to operating temp for at least 1 hour. The heat from the engine will finish curing the parts at 750F or higher.
*Regardless of cure method, do not place parts in an already heated oven as it will cause solvent pop.
NOTE:PLEASE CHOOSE UPS AS SHIPPING METHOD. WE CANNOT SHIP USPS ON CHEMICALS.